Материал устойчивого к износу слоя в карбиде хрома карбида 5+5
Alloy Composition The wear-resistant layer is made from a high-chromium alloy.Its composition includes: Углерод (С): О 5.0% Хром (Кр): 27–30% A martensitic base with a high volume of Cr₇C₃ carbides, восполнение 60% структуры. Hardness Alloy layer hardness: HRC 57–65 Carbide hardness: HV 1400–1800 These values ensure high resistance to...