ASTM規格
ASTM 規格は、パイプなどの材料の製造プロセスと化学組成を定義するために使用されます。, 継手, and flanges. These standards assign “グレード” to indicate specific chemical properties, such as the percentages of carbon, magnesium,
Ex
- Carbon steel pipes: Grade A or
- Stainless steel pipes: Grade TP304 or
- Carbon steel fittings: Grade WPB
Ch
Below are examples of ASTM grades and their chemical requirements:
- Flanges: ASTM A182 (Grades F304, F304L, F316L)
- パイプ: ASTM A312 (Grades TP304, TP304L, TP316L)
- Fittings: ASTM A403 (Grades WP304, WP304L, WP316L)
さらに, you will find a table summarizing commonly used ASTM grades for pipes, 継手, フランジ, valves, bolts, and nuts grouped by their applications.
Special Note on ASTM A105
ASTM A105 does not include a grade designation. Sometimes, the term A105N 使用されています. の “N” does not signify a grade but refers to normalizing, a heat treatment process for ferrous metals. Normalizing helps relieve internal stresses caused by heat treatment, casting, or forming.
CHEMICAL REQUIREMENTS COMPOSITION, %
| Flanges ASTM A182 | ||||||||
| 学年 | C | ん | P | S | そして | で | Cr | モー |
| F304 | 0.08 | 2 | 0.045 | 0.03 | 1 | 8 – 11 | 18 – 20 | |
| F304L | 0.03 | 2 | 0.045 | 0.03 | 1 | 8 – 13 | 18 – 20 | |
| F316L | 0.03 | 2 | 0.045 | 0.03 | 1 | 10 – 15 | 16 – 18 | 2 – 3 |
| 注記: Grades F304, F304L, and F316L shall have a maximum Nitrogen content of 0.10%. |
||||||||
| Pipes ASTM A312 | ||||||||
| 学年 | C | ん | P | S | そして | Cr | で | モー |
| TP 304 | 0.08 | 2 | 0.045 | 0.03 | 1 | 18 – 20 | 8 – 11 | |
| TP 304L | 0.035 | 2 | 0.045 | 0.03 | 1 | 18 – 20 | 8 – 13 | |
| TP 316L | 0.035 | 2 | 0.045 | 0.03 | 1 | 16 – 18 | 10 – 14 | 2 – 3 |
注記:For small diameter or thin walls or both, where many drawing passes are required, a Carbon maximum of 0.040% is necessary in grades TP304L and TP316L. Small outside diameter tubes are defined as those less than 0.50 で. [12.7 mm] in outside diameter and light wall tubes as those less than 0.049 で. [1.20 mm] in average wall thickness (0.044 で. [1.10 mm] in minimum wall thickness). |
||||||||
| Fittings ASTM A403 | ||||||||
| 学年 | C (1) |
ん (1) |
P (1) |
S (1) |
そして (1) |
で | Cr | モー |
| WP 304 | 0.08 | 2 | 0.045 | 0.03 | 1 | 8 – 11 | 18 – 20 | |
| WP 304L | 0.03 (2) | 2 | 0.045 | 0.03 | 1 | 8 – 12 | 18 – 20 | |
| WP 316L | 0.03 (2) | 2 | 0.045 | 0.03 | 1 | 10 – 14 (3) | 16 – 18 | 2 – 3 |
注意事項:(1) 最大, unless otherwise indicated. |
||||||||
FREQUENTLY USED ASTM GRADES
| 材料 | パイプ | Fttg | Flg | バルブ | Bolts そして Nuts |
| 炭素鋼 | A106 Gr A | A234 Gr WPA | A105 | A216 Gr WCB | A193 Gr B7 A194 Gr 2H |
| A106 Gr B | A234 Gr WPB | A105 | A216 Gr WCB | ||
| A106 Gr C | A234 Gr WPC | A105 | A216 Gr WCB | ||
| 炭素鋼 Alloy High-Temp |
A335 Gr P1 | A234 Gr WP1 | A182 Gr F1 | A217 Gr WC1 | A193 Gr B7 A194 Gr 2H |
| A335 Gr P11 | A234 Gr WP11 | A182 Gr F11 | A217 Gr WC6 | ||
| A335 Gr P12 | A234 Gr WP12 | A182 Gr F12 | A217 Gr WC6 | ||
| A335 Gr P22 | A234 Gr WP22 | A182 Gr F22 | A217 Gr WC9 | ||
| A335 Gr P5 | A234 Gr WP5 | A182 Gr F5 | A217 Gr C5 | ||
| A335 Gr P9 | A234 Gr WP9 | A182 Gr F9 | A217 Gr C12 | ||
| 炭素鋼 Alloy Low-Temp |
A333 Gr 6 | A420 Gr WPL6 | A350 Gr LF2 | A352 Gr LCB | A320 Gr L7 A194 Gr 7 |
| A333 Gr 3 | A420 Gr WPL3 | A350 Gr LF3 | A352 Gr LC3 | ||
| Austenitic ステンレス 鋼鉄 |
A312 Gr TP304 | A403 Gr WP304 | A182 Gr F304 | A182 Gr F304 | A193 Gr B8 A194 Gr 8 |
| A312 Gr TP316 | A403 Gr WP316 | A182 Gr F316 | A182 Gr F316 | ||
| A312 Gr TP321 | A403 Gr WP321 | A182 Gr F321 | A182 Gr F321 | ||
| A312 Gr TP347 | A403 Gr WP347 | A182 Gr F347 | A182 Gr F347 | ||
| 材料 | パイプ | Fttg | Flg | バルブ | Bolts そして Nuts |